On Thu, May 15, 2014 at 12:41 AM, James bitsyboffin@... wrote:

> Dynamask film is harder to get and significantly more expensive.
>
> Unfortunately nobody in China, and I mean NOBODY in China, seems to sell Dynamask (or any similar dry film soldermask), while dry film resist is everywhere. 

Interesting.  What about the liquid stuff?  I have seen an application technique where you put a dollop in the center of your board, cover it with a piece of cellophane, and then squeegee it out to the edges.  I don't even think you need to wait for it to dry, you expose it right through the cellophane.

-p.