Archive of the former Yahoo!Groups mailing list: Homebrew PCBs
Subject: Kepping Your Etchant Good? Multiple Use? Muriatic Acid / H2O2
From: "dubob4432" <dubob4432@...>
Date: 2012-10-28
I have been using H2O2 from the pharmacy / Muriatic Acid combo, 2:1 - works well and is easy to get, but it doesn't work after the initial use. It seems every etch, I need to make a new batch. The etchant turns into a bright lime green color on the first etch and it does what I need to pretty quick and it seems like there is decent activity - bubbles which only happens on the first time use, after that maybe bubbles when I first put in the pcb/Cu but they go away very quickly.
After use, I will put the solution in a clear, sealed glass container and even if I use it the next day, after I start, 45min later my etch is still not done, so I dispose of it and make a new batch at which time I am done in 15mins.
What am I doing wrong or where is the mixture out of balance? Again, I just did an etch this evening and had to make a new batch, which is now a bright lime green color.
Thanks in advance,
Bob