--- In Homebrew_PCBs@yahoogroups.com, "sailingto" <sailingtoo@...> wrote:
>
> Does anyone have problems getting large ground plane areas to stay good 'n solid with copper? I've been having a bit of problem with large ground plane areas using toner transfer method. If I do a board without a large ground plane, the traces look good - trace size ranges from .015" to .050" or so.
>
> I clean copper good, wash with alcohol. Toner transfer at 360ºF with a laminator using Pulsar toner transfer paper, then etch in HCl and H2O2. I used the green film last board and it seems a bit better, but not sure about large areas yet.
>
> Just checking to see if anyone else has this problem, or maybe found a solution...... or maybe it's just me?
>
> Thanks for any guidance and suggestions.
>
> Ken H>
>

I thought the Green TRF from Pulsar is designed to fix this exact problem?