Subject: Re: [Homebrew_PCBs] Etchant Temperature

From: Adam Seychell <adam_seychell@...>
Date: 2003-10-14

In general most chemical reaction rates double every 10
degrees centigrade increase. Not sure if this applies to
ferric chloride etching. I remember CuCl2 bubble etching
taking some 30 to 40 minutes minuets to chew through 1 oz
copper at 8°C.


Moore wrote:
> What temperature does Ferric chloride need to be heated too for
> improved etch times?
>