--- In Homebrew_PCBs@yahoogroups.com, "hal91k" <chemistrypaul@...> wrote:
>
> Well, true. But I believe you get a thinner, more consistent finish with this stuff. Here's a photo of the board I did.
>
> http://img511.imageshack.us/img511/2299/pcb006.jpg
>

You definitely get a better plating by using a electroless Tin
plating. Using solder and an iron produces a bit of waviness or
bumpy surface (not to mention the flux which needs to be scrubbed
off). The elctroless Tin plating results in a very smooth layer.

I used to have the recipe for a wonderful electroless Tin plating
solution based on Stannous Chloride, Sodium Chloride, and Sodium
Cyanide. Now that I'm older and wiser (and still alive), I no longer
use that particular material.