On Mon, 08 May 2006 17:00:34 +0200, mycroft2152 <mycroft2152@...>
wrote:

> Any suggestions for temperature in an oven or on a hotplate?
>
>
> Can you resuse the excess afterwards?
>
>
> Myc


I have only tried a couple of times with a hot air gun and don't remember
the temperature.

Didn't try to use the excess, but may be possible if rehydrated.

The procedure is usually too much work for me.
I want instant PCBs ;-)