--- In Homebrew_PCBs@yahoogroups.com, Adam Seychell <adam_seychell@y...> wrote: > The sodium silicates are alkaline, so any contact from acidic > copper etchants will only neutralize and you end up with a > solution of silica gel (colloidal SiO2) and the salt. adam are you telling me that even if the water glass is set and hard the acids wiil desolve it?. i have been advised that gycol and water glass will also harden if mixed, will the acids soften this combo also?. i was toying with the idea of coating the pcb with water glass and print with glycol. or maybe the other way around, coating with gylcol and printing with water glass. there just has to be a better way. mebo