In a message dated 2/13/2013 1:54:36 A.M. Eastern Standard Time, scubadogct@... writes: Does the addition of Hydrochloric acid help to maintain its working strength also? From what I have read adding Hydrochloric Acid (muriatic acid) does help to rejuvenate the Ferric Chloride. Here is a short article on the subject : http://users.monash.edu.au/~ralphk/etching-pcb.html The article says you can rejuvenate Ferric Chloride by adding a small wad of steel wool, then filter out the solution and add some Hydrochloric Acid. The steel wool precipitates the copper out of the solution. It doesn't say how much steel wool to add or how much Hydrochloric Acid to add so you will probably need to do it by trial and error, but should be worth a try. 73 Todd WD4NGG
Message
Re: [Homebrew_PCBs] Re: ferric chloride question
2013-02-13 by toddroberts2001@...