>... >HCl/H2O2 is very fast anyway, but it could probably be useful for CuCl2. > >Leon -=-=-=- I found it not so fast. I etched a 5" x 10" 1-sided board (consisting of several duplicate small circuits) and it took almost an hour. I started with a fresh batch, just enough etchant to cover the board but added more as time dragged on. Maybe my mix is wrong? I'm using 15 percent hcl (muriatic acid) and 3 percent h2o2 at a mix of 1:1. What mix are you using? Thanks, Dave
Message
Re: [Homebrew_PCBs] Sponge etching with HCl and H2O2?
2011-11-26 by DaveC