18u etches faster than 35u, less time, less undercutting. I use mostly 18u simply because it is the material used by the pro board houses (which they then plate up to 35u), and I got it cheap as cutoffs. ST On Sun, Sep 5, 2010 at 8:25 PM, Steve Maroney <steve@...> wrote: > Dear Gang > > > > Do you guys prefer 1oz copper clad over 1/2 oz ? My initial thoughts > is the at 1oz is sturdier and can tolerate heat better than 1/2 ?!? > Please share you experiences. Thanks. > > > > > > > > Best Regards, > > Steve Maroney > > > > Business Computer Support, LLC > > Mobile Phone:504-914-4704 > > Office Phone: 504-904-0266 > > Fax: 866-871-7797 > > > > > > > > [Non-text portions of this message have been removed] > > > > ------------------------------------ > > Be sure to visit the group home and check for new Links, Files, and Photos: > http://groups.yahoo.com/group/Homebrew_PCBsYahoo! Groups Links > > > >