--- In Homebrew_PCBs@yahoogroups.com, lists <Stuartlists@...> wrote: > > In article > <40B5325EDFC7D64F83DC128117C0AD2325AD55@...>, > Jim Barnes <jim@...> wrote: > > Could it be that the Liquid Tin-coated pad is less solderable than bare > > copper? > I've found the same thing so stopped using it. On small boards, I just hand tin with solder or solder paste. It's not the prettiest but it protects the copper and provides solderability. Tuck