Seems you are right one would need to use tin/lead. Some sources say sulphuric acid / peroxide attacks tin. Well, one would have to dig out the discussion from a few years ago to see the details. ST On Fri, Jan 8, 2010 at 2:03 PM, Simao Cardoso <simaocardoso@...> wrote: > Stefan Trethan wrote: >> >> I didn't understand what you are saying there. Anyway I made it plenty >> clear that my information about this etchant is very thin indeed. > > Ohh sorry it's obviously nothing personal, but you mentioned at least 2 > times recently that sulfuric etchants won't etch tin. I don't know much > about this, but i also never saw any prove to that. > >
Message
Re: [Homebrew_PCBs] Dry film tenting problem & pattern plating
2010-01-08 by Stefan Trethan