On Wed, Jan 6, 2010 at 4:09 AM, Stefan Trethan <stefan_trethan@...> wrote: > > > > Hi, > > I think only the sulphuric acid / hydrogen peroxide etchant will work > with tin as reisist. > It is similar to CuCl but has the disadvantage of not keeping as well, > requiring more maintainance. > > I think gold would work as a resist for the other etchants, but is > slightly more expensive ;-) > > ST Hi Stefan, I've been working CuCl etchant recently and really had problems with the terrible fumes it puts off, particularly when it's heated so it will actually etch a board. Can you explain a little about the disadvantages of Sulfuric/Peroxide etchant and how to maintain the etchant bath? Sulfuric acid seems so much less harsh when it comes to fumes and I would like to try it. Do have any suggestions for the concentrations or PH of the solution to make it work? Thanks- Larry