Re: [Homebrew_PCBs] Tin - Plating

2008-06-04 by JanRwl@AOL.COM

In a message dated 6/3/2008 6:02:58 P.M. Central Daylight Time,  
dj@delorie.com writes:

I just  soak the board in Liquid Tin (MG Chemicals) for a few  minutes.<<
Doesn't that solution have to be warm (say 140°- 280° F or more) to work  
well?        Jan Rowland