At 01:03 AM 5/20/2008 -0400, DJ Delorie wrote: > Plus, you can buy HCl and H2O2 cheaply, whereas FeCl is getting harder > to find locally and more expensive. I was trying to find some FeCl for etching brass, but with a dozen Radio Shack stores in this town, none of them had it in stock. Later I happened to be in an art supply store (the Dick Blick chain) and found they carried it for about $4/pint (about half the price I rememeber Radio Shack charging). In addition to etching its used for getting a patina on metals, so another source might be a store that caters to stain glass artists who want that old antique look on the metal parts of their work. Mike P.S. - But for PCB work, count my vote for that pretty emerald green CuCl.
Message
Re: [Homebrew_PCBs] H2O2 + muriatic acid etchant?
2008-05-21 by Mike Schoenborn