Leon wrote:
ferric chloride or persulfate etchants. Just limit it to 20 seconds
between stirring. No need to waste your time with hot water baths.
I have to agree that manual agitation has its benefits.
>For small volumes ( < 1L ), you can use microwave oven to directly heat
> I bought a bubble etch tank, tried it once, then went back to manual
> agitation with a plastic container holding the etchant inside a larger
> container with some hot water in it.
>
> Leon
>
>
ferric chloride or persulfate etchants. Just limit it to 20 seconds
between stirring. No need to waste your time with hot water baths.
I have to agree that manual agitation has its benefits.