--- In Homebrew_PCBs@yahoogroups.com, DB Express <dbxprss@...> wrote: > > I just etched my PS board this morning. Not too bad for a first try: > http://members.lsol.net/gop4evr/unlinked/psboard.jpg > > I used homebrew etchant (2:1 hydrogen peroxide/muriatic acid). At $2.69/gallon for the muriatic acid and 69 cents/quart for hydrogen peroxide, this sure beats paying $6/pint for the FeCl. It works well, but has some odor. I used it outside just as an extra precaution. > If I may go off topic on the side of safety and household hazzards. As you probably found out, the chemicals you used were rather good at removing metal. What you may soon find out, they are SO good, that EVERYTHING metal in the room in which they are kept will start to rust. stuff across the basement and inside of wooden boxes. I took my Muriatic Acid, sold as such to etch stone and clean concrete, and I put that into a 5 gallon bucket with a lid that had an O-ring of silly-cone. Dave