I tried around with it most of the day. The ink doesn't seem to resist fully and properly. I even tried FeCl, but the stain in a bottle shows even more damage/under-etching than CuCl. (BTW: many year old FeCl already mixed in a PET bottle is still good, and i discovered the vacuum sealed PE bags of FeCl powder/granules have let through enough water to wet it slightly. that stuff must be hygroscopic like crazy.) I've started a wiki here which gives me lotsa easy-upload space for pics (200Mb) <http://dipcb.schtuff.com/?action=gallery&q=pcb> I hope you have permisson to view as-is, let me know if not. Basically the etchant etches through and i do not know why. Anyway, i'd thought i throw that at you guys for ideas. Volkan, is there a way to measure at which temperature and how long you cure? ST