On Tue, 06 Jun 2006 08:51:03 +0200, Andrew <andrewm1973@...> wrote: > > HOWEVER - if you only etch one board in a > blue moon - Amonia Persulphate or FeCl are > probably better ideas. I wouldn't even be sure of that. There's no disadvantage of CuCl that i can see, so why would the others be better? As long as you have enough spare space to store your tank and two bottles of regenerating chemicals it really seems a good etchant. Of course if one can get the other etchants easier.... ST
Message
Re: [Homebrew_PCBs] Re: Ammonium Persulphate
2006-06-06 by Stefan Trethan