Anyway, i bought the more expensive silver paste because it must surely be better ;-) BUT, it seems to reflow in the same strange manner as the leaded paste. When you heat it until it has a dry, grayish appearance, and then wipe it off, it will come off as sort of dried paste/powder, BUT the board will be tinned in a thin, shiny layer. When you heat it further, until it reflows, it will get a dull, rough appearance from where the particles melted. I don't understand the first thing. How can it tin the board without melting, at all? What happens? ST
Message
Re: [Homebrew_PCBs] Re: Tinning the board? - reflow
2005-11-21 by Stefan Trethan