Re: [Homebrew_PCBs] Uneven etching problem

2005-07-21 by Leon Heller

----- Original Message ----- 
From: "Stuart Wallace" <stuartw@...>
To: <homebrew_pcbs@yahoogroups.com>
Sent: Thursday, July 21, 2005 4:59 PM
Subject: [Homebrew_PCBs] Uneven etching problem


> Hi,
>
>
> Bit of a ramble -- sorry about this...
>
> I've recently developed a bit of a problem with my etching process and
> I'm hoping that someone can give me some suggestions for improvement.
>
> Up to now I've been etching FR2 boards at roughly 10/10 (10 mil tracks,
> 10 mil spaces) with good yield. I've recently moved to FR4 substrate and
> 8/8 rules in order to make a board for a slightly higher-speed design,
> and yield has now dropped to zero. I've uploaded a couple of pictures of
> my latest effort -- they were taken with a camera phone so they may not
> be very useful. I have been experimenting with UV exposure times: the
> top side of the board was exposed for 2 mins 45 secs; the bottom side
> for 2 mins 30 secs. I normally expose for 2 mins 15 seconds but this
> doesn't seem like enough for the FR4 board.

I get boards looking like that when I use old PCB stock. The resist is only 
good for six months or so after it has been applied.

Leon 



-- 
No virus found in this outgoing message.
Checked by AVG Anti-Virus.
Version: 7.0.323 / Virus Database: 267.9.2/53 - Release Date: 20/07/2005

---
[This E-mail has been scanned for viruses but it is your responsibility 
to maintain up to date anti virus software on the device that you are
currently using to read this email. ]

Attachments

Move to quarantaine

This moves the raw source file on disk only. The archive index is not changed automatically, so you still need to run a manual refresh afterward.