On Sat, 12 Mar 2005 16:33:07 -0000, Leon Heller <leon.heller@...> wrote: > > I just checked Delrin's properties, it's no good in acid or alkaline > solutions: > http://www.upchurch.com/TechInfo/matDelrin.asp > It's a pity, as it's otherwise a very good material. > Thanks a lot. I especially like that: " It is best to use Delrin with neutral pH aqueous solutions or organic solutions for guaranteed best performance." As if i could choose the liquid to suit their plastic, silly people... >> >> >> I also would have a carbon fiber tube from model building with 8mm dia >> for >> a shaft that could easily take the load, but i don't know how i would >> make >> the bearing if i use that. It is carbon fiber in some resin, probably >> epoxy, wall thickness is about a mm. > Carbon fibre uses a similar epoxy resin to fibre-glass. > Leon Seems so. But i have not the slightest idea how i could make bearings for the carbon fiber tube... ST