Hi Phil, I got it from an internet chemical supplier, along with the acid and copper oxide. Their minimum order is something like 50UKP so it is not practical to just get the H2O2 from them. Les Phil wrote: > --- In Homebrew_PCBs@yahoogroups.com, Les Newell <lesnewell@f...> wrote: > >>Hi Phil, > > ... > >> A teaspoon of >>100volume H2O2 is enough to get it etching well again. If the solution >>starts fizzing when you add the H2O2 and has a chlorine smell you have >>added too much. >> >>Les > > > Thanks, Les. Where did you get your H2O2? > > Phil > > > > > Be sure to visit the group home and check for new Bookmarks and files: > http://groups.yahoo.com/group/Homebrew_PCBs > Yahoo! Groups Links > > > > > > >
Message
Re: [Homebrew_PCBs] Re: advice on CuCl etchant?
2004-09-28 by Les Newell