Thanks for all the suggestions - the solution is not olive at all. It appears to be a clear, bright green. I would have called it "lime green" but its not far from emerald. So it looks like I need to find some concentrated H2O2. Anyone know a source in the Seattle area? By the way, I think there was some etching going on - the surface of the copper took on that characteristic flat texture you get when etching first starts. Of course, this was after 45 minutes... sigh... Phil
Message
Re: advice on CuCl etchant?
2004-09-28 by Phil