On Sun, 19 Sep 2004 22:53:27 -0000, Phil <phil1960us@...> wrote: > > Thanks Stefan. This is the first time I've heard not to use a heater. > I recall reading somewhere to heat the CuCl solution so its a little > confusing. I looked for the page that said that but couldn't find it > since I didn't bookmark it. It might have been one that talked about > using CuCl salt, though. > > I guess technically, this is HCl etching at first and then CuCl. > > A How-To for HCl and H2O2 etching would be very useful. > > Phil > you are right there, first Cl only, then CuCl. the heating is no good. only a little is possible and that isn't helping much. HCl vapor is bad business, very bad. Tomorrow i will try using pool-supply Clorine to regenerate. curious and have a pool. 'night. ST
Message
Re: [Homebrew_PCBs] Re: CuCl questions
2004-09-19 by Stefan Trethan
Attachments