Yahoo Groups archive

Homebrew_PCBs

Archive for Homebrew_PCBs.

Index last updated: 2026-03-30 01:05 UTC

Message

Re: [Homebrew_PCBs] Re: plated tin as the etch resist

2004-04-02 by Jeremy Taylor

Thanks for the tip - I'll mix some up tomorrow morning, and err... figure
out a place to put the new pre dip .

JT

http://www.soundclick.com/jtsound

<snip>
> If you dip the tin-lead plated panels in straight peroxide (30% or
> stronger) for 15 or 20 seconds
> Tom

Attachments