Anyone tried using Rayzist film?

2004-03-22 by Steve Greenfield

I have to investigate this more... it looks like a photosensitive
film that "develops" in water, and sticks down without heat.

It is made for sandblast etching/carving. But if the hardened film
stands up in water, perhaps it could be used for acid etching.

http://www.rayzist.com

Steve