Yes my very thoughts , I still use the old method with granules so its no go for me, hardly worth the hassle, shall give the whole Idea a miss. When projects finished give PCB a nice clean then spray with PVC to keep the copper shining , also a good insulator, so does two jobs. ________________________________ From: fred27murphy <fred27murphy@...> To: Homebrew_PCBs@yahoogroups.com Sent: Monday, 19 August 2013, 12:52 Subject: [Homebrew_PCBs] Re: silver coating If tining before etching works well, I wonder why you don't see pre-tinned copper clad boards? I suppose it limits you choice of etchant. [Non-text portions of this message have been removed]