I guess I don't know what "tenting" means. -- Phil M. ----- Original Message ----- From: "cunningfellow" <andrewm1973@...> To: <Homebrew_PCBs@yahoogroups.com> Sent: Wednesday, May 22, 2013 8:13 PM Subject: [Homebrew_PCBs] Re: printer >> Phil wrote: >> >> I haven't measured the film, but I'd guess >> about 1 or 2 mils thick. > > 33um (1.3 mil inch) is the thickness of stuff > that the manufacturer of the stuff I use says > is unsuitable for "tenting" > > 50um (2 mil inch) is listed as good for tent > > So 1..2 mil could make a difference. > > I nice high contrast phototool makes a diff > too. Getting the tent all UV'd up before the > develop step. > > > > ------------------------------------ > > Be sure to visit the group home and check for new Links, Files, and > Photos: > http://groups.yahoo.com/group/Homebrew_PCBsYahoo! Groups Links > > >
Message
Re: [Homebrew_PCBs] Re: printer
2013-05-23 by Phil@Yahoo