On 12/05/2013 15:07, dave_donlan wrote: > Hi guys > I am using UV exposure method on clear acetate > > 15 secs exposure caustic soda developer about a 60 secs > > hydrochloric acid / peroxide etchant no bubbler just sloshing about but > the problem is the protective layer is coming off after a few minuets of > etching > > hydrochloric is 30% > peroxide is 9% Use a test strip with a range of exposure times to get the correct exposure. Leon -- Leon Heller G1HSM
Message
Re: [Homebrew_PCBs] photo layer coming off
2013-05-12 by Leon Heller