2013-05-12 by dave_donlan

Hi guys 
I am using UV exposure method on clear acetate

15 secs exposure caustic soda developer about a 60 secs

hydrochloric acid / peroxide etchant no bubbler just sloshing about but the problem is the protective layer is coming off after a few minuets of etching

hydrochloric is 30%
peroxide is 9%

Any advice please