Jeff, It is almost always the case that a pressure specification is in "psi"--pounds per square inch. With paid, the board could be and inch wide or a foot and it wouldn't matter. 73, Todd On Jan 20, 2013 1:46 PM, "Jeff" <jeff.heiss@...> wrote: > ** > > > For laminating dry film photoresist to copper clad, the datasheet for > Riston film says to use a laminator roller pressure of 40 pounds but it > does not state the width of the board which is needed for lb/in. If the > width of the board for 40 pounds is 12 inches, then a 6 inch wide board > would use 20 pounds. > > Do the experienced have any hints for roller pressure? > > Jeff > > > [Non-text portions of this message have been removed]
Message
Re: [Homebrew_PCBs] laminator roller pressure for dry film
2013-01-21 by Todd F. Carney