"poofjunior" <seeifyoucanmeetme@...> writes:
I'm still using it. I run the air pump only when I'm actively using it
(i.e. from "plug in the heater" to "done"), and it's been jade green the
whole time. I occasionally test the HCl levels and add acid, and/or let
some of the water evaporate, but otherwise I just use it to etch.
and air pump.
> Has anyone had any long-term success with this process? How long doesI put together my CuCl etchant around March 2008, so four years ago.
> it take to aerate? Is there any excess waste that needs to be dumped
> eventually?
I'm still using it. I run the air pump only when I'm actively using it
(i.e. from "plug in the heater" to "done"), and it's been jade green the
whole time. I occasionally test the HCl levels and add acid, and/or let
some of the water evaporate, but otherwise I just use it to etch.
> Are there any circuits I can create to duplicate an electrolysisThere's no electricity involved in my tank at all, aside from the heater
> setup?
and air pump.