Yahoo Groups archive

Homebrew_PCBs

Index last updated: 2026-03-31 23:13 UTC

Message

Re: [Homebrew_PCBs] FR-4 Copper Clad and Etchant mix

2011-02-22 by Tom Biery

I don't know if that formula is correct I am curious if it is? What are the
benifits of using that vs ammonium persulfate, that is what I am using in this
youtube video... http://www.youtube.com/watch?v=trnvlrVq6P0%c2%a0and it works fine.

Please let me know.
Tom




________________________________
From: Randy S. <rj3819@...>
To: Homebrew_PCB <homebrew_pcbs@yahoogroups.com>
Sent: Mon, February 21, 2011 8:29:51 PM
Subject: [Homebrew_PCBs] FR-4 Copper Clad and Etchant mix


FR-4 doesnt have to be green colored? Correct ?

Other question .. for making etchant ..
I saw 2 parts peroxide to one part muriatic acid ( 34% hydrochloric acid )
and I saw 3 to mix as well ..
Is it crucial ? I mean I guess the only thing that it would change is the
etching
times .. and the fumes LOL .. ??

Randy




[Non-text portions of this message have been removed]