Re: Quick kapton and copper foil flex circuit test

2010-07-14 by javaguy11111

--- In Homebrew_PCBs@yahoogroups.com, Tony Smith <ajsmith@...> wrote:
>
> > Heat seal flex sounds interesting, but I do not see any places that sell it.
> >
> > I did find a place that sells hot melt powder, but none of their
> > distributors seem to sell it.  The site is
> 
> > http://www.lancergroup.com/lancer/ink_catalog/additives_bases/catalog5b.html
> >
> > It is the H-10 powder. I have sent them email to find out who carries it.
> 
> 
> Try a scrapbooking / art craft shop.
> 
> They sell 'embossing' powder which sounds like that stuff.  That has a fairly
> low melt temperature.
> 
> Tony
>
Thanks. Found the adhesive powder online at advancedscreen.com and some 325 mesh copper powder at chemicalstore.com. So I guess I will be doing some experimenting after all.