Re: [Homebrew_PCBs] Re: Old GL FeCl -very slow etching copper

2010-05-18 by mlerman@ix.netcom.com

-----Original Message-----
>From: Ben L <bhleavi@...>
>Sent: May 17, 2010 11:55 PM
>To: Homebrew_PCBs@yahoogroups.com
>Subject: [Homebrew_PCBs] Re: Old GL FeCl -very slow etching copper
>
>
>
>> I found cupric chloride to be very slow at room temp, it benefits from heating even more than FeCl. HCl + peroxide certainly works fine at room temp though, until enough of it converts.
>>
>
>I have never heated mine before. In fact I have it on the back porch and have etched boards fine in cold weather. I just pump lots of air into it. Sometimes add a little HCl if it seems to be slower than normal. I kept it covered when not in use but can still vent. So times will leave it uncovered to reduce it down some. I normally don't add any peroxide.
>
>Ben
>

How long does a board take to etch with this system?

Mark




>
>------------------------------------
>
>Be sure to visit the group home and check for new Links, Files, and Photos:
>http://groups.yahoo.com/group/Homebrew_PCBsYahoo! Groups Links
>
>
>