"cunningfellow" <andrewm1973@...> writes: > A 60 second exposure with a UV tube will give harder edges to the > resist than a 10 minute exposure with a lower intensity source. Would this affect etch-under at all? My latest board had trace thinning to the point where many were missing completely, I've been "bloating" my films to compensate but a better process would be a better solution.
Message
Re: [Homebrew_PCBs] Re: LEDs versus tubes
2010-01-29 by DJ Delorie