"Herbert E. Plett" <cachureos@...> writes: > perhaps a little more HCl is needed, it also fumes out... Follow-up: CuCl concentration is below 1.2 (which I figured). Acid seems high enough. I heated some copper wire to get Copper Oxides, and the etchant dissolved that just fine, leaving a bright pinkish copper behind. I did that a few times to get more copper into the tank, and then left the wire in there. Perhaps by the time I get around to fiddling with it again it will be more usable, otherwise I'll put in more H2O2. I did make up some NaOH solution for titration but it neeeds time to fully dissolve.
Message
Re: [Homebrew_PCBs] sluggish etchant
2008-06-18 by DJ Delorie