Yahoo Groups archive

Homebrew PCBs

Index last updated: 2026-04-03 01:13 UTC

Message

Re: [Homebrew_PCBs] sluggish etchant

2008-06-17 by Leon

----- Original Message ----- 
From: "DJ Delorie" <dj@...>
To: <Homebrew_PCBs@yahoogroups.com>
Sent: Tuesday, June 17, 2008 8:52 PM
Subject: Re: [Homebrew_PCBs] sluggish etchant


>
> "Leon" <leon355@...> writes:
>> What concentration is the H2O2 you are using?
>
> It was the usual 2 parts 3% H2O2 to 1 part 37% HCl.  But like I said,
> it's been sitting for a while.

3% is too weak, unless you make up fresh etchant each time. I use ferric 
chloride, it's much less trouble.

Leon
--
Leon Heller
Amateur radio call-sign G1HSM
Yaesu FT-817ND and FT-857D transceivers
Suzuki SV1000S motorcycle
leon355@...
http://www.geocities.com/leon_heller