> Thanks Peter for the MG Chemicals link. This sounds like it is worth trying. > Tinnit and the other similar solutions usually only last for a one time > plating. I use Tinnit too. Works great. Just dip an etched board with clean copper traces in Tinnit for two minutes and it's zinc plated, protected and easy to solder! I keep it in a wide necked Rubbermade container and dip small boards in from the top. - Chris Graham
Message
Re: [Homebrew_PCBs] Tin plating...
2003-05-21 by Chris Graham