Yahoo Groups archive

Homebrew PCBs

Index last updated: 2026-04-05 19:38 UTC

Message

No more going to Radio Shack - First attempt with Muriatic Acid GOOD!

2007-04-11 by izzo47

Went to 3 RS for Ferric chloride all OUT....
Reading old msgs, I finally found that Lowe's had it, a Gal was 7 bucks.
I bought some regular 3% Hydrogen Peroxide. It work well and fast but 
would like any feed-back on the recipe I used.
 1 part (200ml) 31.45% Muriatic Acid, 2 parts (400ml) Peroxide. Color 
was light green, No heat used. Board went in first, pour the 400ml of 
Peroxide on the board and in about 6 minutes it was done (small test 
board) 3x2 inches. I did get a little scared when I measured the 400ml 
of Peroxide in the same plastic cup as there maybe was a drop of the 
Acid still in there and saw smoke/vapors for a second. I noticed that 
during the clean-up with water it turns a nice light blue, natural I 
guess?
Question is the recipe OK? Can it be fine-tuned.
Can it be saved and brought back to life to use again? 

BTW if you can get your hands on the green tape they use at Wal-Mart in 
the Photo Dept to attach leader cards that go through the film 
processor, get some. It will not melt or leave any residue I am sure of 
that as a friend that works there gave me a roll.

Attachments

Move to quarantaine

This moves the raw source file on disk only. The archive index is not changed automatically, so you still need to run a manual refresh afterward.