>Professional PCB suppliers use a different etching chemistry - I think it's
>based on ammonia, it's alkaline, anyway. Perhaps that doesn't affect the
>tin.

I've just checked the above with a web search, and it's basically correct. 
The etchant is ammonia, ammonium chloride and cupric chloride. The excess 
copper needs to be removed regularly. This stuff doesn't dissolve tin or 
tin/lead, unlike FeCl3 and other acidic etchants.

Leon
--
Leon Heller, G1HSM Tel: +44 1424 423947
Email:leon_heller@...
My web page: http://www.geocities.com/leon_heller



_________________________________________________________________
Hotmail messages direct to your mobile phone http://www.msn.co.uk/mobile

Attachments