Luther - thanks for the hydrogen peroxide idea (and thanks to Rolan for this also). I may try it tomorrow since I don't see much change after 24 hours with the lid off the etch tank, except a few more blue spots; maybe ten 1/4" long bits on the many copper wire above acid level. I know someone who is a hairdresser and I think they have access to inexpensive hydrogen peroxide so I'll see what concentration it is and if its cheaper than drug store grade. Grant --- In Homebrew_PCBs@yahoogroups.com, luther m stroud <dukes500@j...> wrote: > I made my cucl like you with copper and hcl . adding some drug store > hydrogen peroxide 3% on the bottle will help get it strarted . the data > on some graphs i was looking at said etch is best at 35c about 2,5 molar > cucl and a saturated with sodium cloride also in that same bath of > etchant. allows you to use less hcl. wonder if you can heat the air > you bubble to warm the solution rather that cool it . good luck with > your etcher project.
Message
Re: Starting CuCl etchant from scratch
2003-04-15 by grantfair2001
Attachments
- No local attachments were found for this message.