On Sat, 06 May 2006 23:27:07 +0200, Leon Heller <leon.heller@...> wrote: > > > Try adding some HCl, that should get rid of the sludge. Adding H2O2 will > > also help, with the HCl it will convert cuprous chloride into cupric > > chloride. Doing that should allow you to use the solution indefinitely, > if > > you wish. Heating to about 50C will speed things up a lot. I always heat > my > > FeCl3 etchant by putting the etchant container inside a larger one > > containing hot water. > > > Leon Do not heat any etchant containing HCl. HCl boils at very low temperature and large amounts of corrosive gas are released even below that. ST
Message
Re: [Homebrew_PCBs] Ferric Chloride - muck at bottom of tank question
2006-05-06 by Stefan Trethan