--- In Homebrew_PCBs@yahoogroups.com, "idaho_huckleberry" <dmiller45@...> wrote: > > What strength of HCL and H2O2 did you use? I went shopping for Muratic > acid and found some at 37%, the H2O2 was 12% (listes as "40" on the > side of the bottle) from my local Salon supply store. Are these stong > enough to etch PCB's or should I look for stronger stuff? > > Dave Miller > You may want to check the 'Files' section of the group. There are a number of very good articles posted there which have the details on the acid etching process. Regards, Bob
Message
Re: HCL + Peroxide Question
2006-03-06 by Bob_xyz