Yahoo Groups archive

Homebrew_PCBs

Index last updated: 2026-03-31 13:47 UTC

Message

Re: [Homebrew_PCBs] Regenerating CuCl

2005-09-02 by Stefan Trethan

On Fri, 02 Sep 2005 02:07:31 +0200, johnwhitneyfiat
<johnwhitneyfiat@...> wrote:

> I have been off the group for a while and I'm sure this was covered.
> In the direction for making etchant from Hydrogen Peroxide and Muratic
> Acid, it says that you can regenerate with a bubbler. How long does
> this take? I know it will depend on the amount and the area that was
> etched, but is there a rule of thumb to make it work. I do have to day
> that I make a small bathch and it worked great on a sample board.
> John Whitney
> Wis X 1/9


I personally never tried it, but i would say many hours, perhaps days.
My tank volume isn't that large, and that means if i run out of active
etchant halfway through a board i have to do something, waiting very long
until it is regenerated is not an option. So i just add a small amount of
CuCl.
With the low price of that stuff and tiny amounts required.....


ST

Attachments