----- Original Message ----- From: "Naveed Alam" <naveedguy2@...> To: <Homebrew_PCBs@yahoogroups.com> Sent: Tuesday, August 09, 2005 12:02 AM Subject: [Homebrew_PCBs] FeCl2 >I have a solution of FeCl2 for etching copper boards. > I keep it in a plastic bottle having a tight cap. > Is there any problem with it. Is there any possibility > that the solution may lose its etching power with > time. > Should I dry it to get the powder? It'll keep as long as you like. BTW, you can etch a board, save the etchant, and reuse it several times. Leon -- Leon Heller, G1HSM leon.heller@... http://www.geocities.com/leon_heller -- No virus found in this outgoing message. Checked by AVG Anti-Virus. Version: 7.0.338 / Virus Database: 267.10.4/66 - Release Date: 09/08/2005 --- [This E-mail has been scanned for viruses but it is your responsibility to maintain up to date anti virus software on the device that you are currently using to read this email. ]