In message <000b01c4f427$b1f3bfe0$f3d3b251@leon1>
"Leon Heller" <
leon.heller@...> wrote:
> I use an Electrolube flux pen (SMF12P) for SM, as the no-residue solder I
> use doesn't have a very active flux.. You don't really need separate flux
> for through-hole parts if you use resin-cored solder.
The Multicore 60/40 tin/lead solder with the "Ersin 362" flux is about the
best I've found. Use a good temperature-controlled solder station (I use an
Antex 660TC) and keep the tip clean. Avoid the Multicore TTC tip cleaners - I
had one decompose into beads of solder and flux. If you get a layer of crud
on your soldering iron tip that a wet sponge won't remove, rub the iron tip
lightly on a piece of wet 600-grit sandpaper or use a small craft knife to
scrape it off.
Later.
--
Phil. | Acorn Risc PC600 Mk3, SA202, 64MB, 6GB,
philpem@... | ViewFinder, 10BaseT Ethernet, 2-slice,
http://www.philpem.me.uk/ | 48xCD, ARCINv6c IDE, SCSI
... Quick! Close your mind!! Something might get in.