Subject: Board surface roughness

From: "gettingalongwouldbenice" <gettingalongwouldbenice@...>
Date: 2004-11-18

I've run into another snag with electrostatic toner transfer.
For fine lines, you want thin copper. But the thin
copper takes on the texture of the underlying fiberglass mat.
So I get holes in the toner.
Photo is 3upclose
Ideas?
mike