> The hydrated form doesn't generate very much heat or splash much.
It
> should be added to the water rather than vice versa. The anhydrous
> form generates more heat. I've never had any problems with either
> type, though.
>
>
> Leon

Interesting. I didn't notice 2 forms being sold. Not that it
matters much as I dont intend to use FeCl unless desperate and I'll
get the pre-mixed stuff from radio shack.

And, yes, I added the dry stuff to the water but it still made a
horrible mess splattering. Even small amounts caused problems. I
did have several years of University Chem so I know the proper
procedures.